| Sign In | Join Free | My futurenowinc.com |
|
Brand Name : Zhonggong Special Metallurgy
Model Number : GH5188 Alloy
Place of Origin : China
MOQ : 100KG
Price : Price is negotiated based on the required specifications and quantity
Payment Terms : Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Ability : 5000 tons per month
Delivery Time : 5-8 working days, depending on the parameters required for negotiation
Packaging Details : Standard export packaging, or packaging as required
Certification : ISO Certificate
Material Type : Nickel-based Superalloy
Chemical Composition : Ni, Cr, Co, Mo, W, Ti, Al, other elements
Density : ~8.4 g/cm³
Tensile Strength : ~1000 MPa
Yield Strength : ~850 MPa
Temperature Range : Up to 980°C (1800°F)
Oxidation Resistance : Excellent
Corrosion Resistance : High
Applications : Aerospace, power generation, chemical processing
GH5188 Alloy is a high-performance nickel-based superalloy specifically engineered for demanding applications where extreme conditions are prevalent. This alloy is characterized by its superior high-temperature strength, excellent resistance to oxidation and corrosion, and robust mechanical properties.
GH5188 Alloy's combination of high strength, thermal stability, and resistance to harsh environments ensures it meets the stringent requirements of advanced industrial and aerospace applications.
Here’s a typical composition table for GH5188 Alloy:
| Element | Composition (%) |
|---|---|
| Nickel (Ni) | Balance |
| Chromium (Cr) | 19.0 - 21.0 |
| Cobalt (Co) | 10.0 - 12.0 |
| Molybdenum (Mo) | 3.5 - 4.5 |
| Tungsten (W) | 3.0 - 4.0 |
| Titanium (Ti) | 2.0 - 2.5 |
| Aluminum (Al) | 1.5 - 2.0 |
| Carbon (C) | ≤ 0.08 |
| Boron (B) | ≤ 0.01 |
| Silicon (Si) | ≤ 0.50 |
| Manganese (Mn) | ≤ 0.50 |
These values are approximate and can vary based on the specific production standards and requirements.

|
|