| Sign In | Join Free | My futurenowinc.com |
|
Brand Name : Zhonggong Special Metallurgy
Model Number : GH3044 alloy
Place of Origin : China
MOQ : 100KG
Price : Price is negotiated based on the required specifications and quantity
Payment Terms : Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Ability : 5000 tons per month
Delivery Time : 5-8 working days, depending on the parameters required for negotiation
Packaging Details : Standard export packaging, or packaging as required
Nickel (Ni) : Balance
Chromium (Cr) : 20.0-22.0%
Iron (Fe) : 5.0-7.0%
Cobalt (Co) : 1.0-2.0%
Density : ~8.4 g/cm³
Melting Point : ~1370°C (2500°F)
Thermal Conductivity : ~10-12 W/m·K
Yield Strength : ~690 MPa (100 ksi)
Ultimate Tensile Strength : ~880 MPa (128 ksi)
Elongation : ~15%
Certification : ISO Certificate
GH3044 Alloy
GH3044 is a high-performance nickel-based superalloy designed for exceptional strength and oxidation resistance in high-temperature environments. This alloy is predominantly used in the aerospace and power generation industries due to its superior mechanical properties and resistance to extreme conditions.
Key Features:
GH3044 alloy's unique combination of strength, temperature resistance, and corrosion resistance makes it a preferred choice for demanding engineering applications, contributing to enhanced performance and extended service life of components.
Feel free to adjust this description based on specific needs or additional features of the alloy you want to highlight.
Here’s a detailed composition table for GH3044 alloy:
| Element | Content Range |
|---|---|
| Nickel (Ni) | Balance |
| Chromium (Cr) | 20.0-22.0% |
| Iron (Fe) | 5.0-7.0% |
| Molybdenum (Mo) | 4.0-5.0% |
| Tungsten (W) | 0.5-1.5% |
| Cobalt (Co) | 1.0-2.0% |
| Aluminum (Al) | 0.8-1.2% |
| Titanium (Ti) | 1.0-2.0% |
| Boron (B) | 0.005-0.015% |
This table provides a clear overview of the alloy's chemical composition, crucial for understanding its performance characteristics.


|
|
GH3044 alloy is a nickel-based superalloy with high strength and oxidation resistance. Images |